MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Eastman Provista NXT Copolymer Resin for Profile Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Applications:
  • Candy packaging
  • Corner guards
  • Displays, Fixtures and Point of purchase
  • Food packaging
  • Furniture guards
  • Integrated circuit tubes
  • Lighting tubes
  • Plastics for hygiene feminine products
  • Pricing channels
  • Teething rails
  • Tubing

Key Attributes:

  • Capable of running on PVC lines with minor setup adjustments
  • Compatible with the PET recycle stream
  • Good chemical resistance
  • Good melt strength with ease of handling
  • Good toughness with design flexibility
  • High processing speeds
  • Sparkling clarity with high gloss
  • Versatile process setup (high or low drawdown ratios, multiple cooling methods)

Product Description: Eastman Provista copolymer NXT is a resin specifically developed for extrusion into profiles where aesthetics like high clarity and gloss, coupled with design flexibility and sustainability drive demand. Compared to commonly used materials, Eastman Provista copolymer NXT can often run on most standard processing equipment at increase speeds. The extremely high melt strength of this resin gives added versatility for a variety of process setups and makes it an excellent choice when extruding profiles into complicated shapes. Its compatibility with the PET recycle stream makes this product and environmentally friendly choice. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®. This product is certified to NSF/ANSI Standard 51 for Food Equipment materials. This product has been CRADLE TO CRADLE CERTIFIEDcm Silver.

Information provided by Eastman.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Density, ASTM D792
  • Linear Mold Shrinkage, ASTM D955
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Unnotched, ASTM D4812
  • Puncture Energy, ASTM D3763, At Max load
  • Puncture Energy, ASTM D3763, At Max load
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, at 45°
  • Transmission, Visible, ASTM D1003, Regular
  • Transmission, Visible, ASTM D1003, Total
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.