MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Description: Research carried out in about the last fifteen years in CREUSOT LOIRE INDUSTRIE laboratories shows that a strong addition of silicon to austenitic stainless steels of the 18/10 type has a favorable influence on resistance to transpassive intergranular corrosion. This type of corrosion develops particularly in very concentrated nitric environments (> 90 %) up to boiling point, also in strongly oxidizing nitric environments (oxidizing ions present such as : hexavalentchromic pentavalent vanadium - ferritic salts etc...). URANUS® S1 steel grade puts in a concrete form the results of research in this domain.

Information provided by manufacturer.

Key Words: EURONORM X1 Cr Ni Si 18.15.4, AFNOR Z1 CNS 17.15, DIN W. Nr 1.4361, ASTM UNS S30600
Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate, Minimum Guaranteed
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio, Calculated
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As remainder
  • Nickel, Ni
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Groupe Arcelor

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.