MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Mercon® V ATF
Categories: Fluid; Lubricant

Material Notes: MERCON® V ATF is a premium quality, synthetic blend transmission fluid approved for use in passenger car and light truck automatic transmissions that require a Ford MERCON® V fluid. It is back serviceable for use in 2006 and earlier model-year Ford vehicles where the OEM previously specified MERCON® fluid, and also may be used in most 2005 and earlier model-year GM automatic transmissions. MERCON® V ATF is formulated to provide improved antiwear and anti-shudder performance compared with previous-generation fluids, as well as better low-temperature properties. It is highly shear stable and has excellent oxidation resistance for long fluid life. The part-synthetic formulation provides enhanced performance benefits compared with conventional, all-mineral transmission fluids.

Applications:

  • Ford automatic transmissions where a MERCON® V fluid or earlier-generation MERCON® fluid (obsolete) is specified
  • GM automatic transmissions in 2005 and earlier vehicles, except those that require a DEXRON®-VI fluid for warranty coverage, or a Type T-IV or CVT fluid
  • Heavy-duty automatic and powershift transmissions in trucks and buses
  • Power steering systems in many newer Ford vehicles
  • Hydraulic systems on industrial and mobile equipment operating over a wide temperature range
MERCON® V ATF is OEM-approved for service fill in the following applications:
  • Ford MERCON® V (License Nos. M5091001, M5091002, M5091003, M5091004, M5091005)
  • Voith DIWA transmissions MERCON® V ATF is recommended for service fill in the following applications:
  • Allison automatic transmissions in off-highway applications where a C-4 quality fluid is specified
  • ZF Ecomat transmissions
Features/Benefit:
  • Proper frictional properties for smooth shifting and excellent anti-shudder performance
  • Excellent oxidation resistance and thermal stability for long fluid life
  • Protects against sludge and varnish formation
  • Protects against wear
  • High shear stability
  • Protects against rust and corrosion
  • Excellent low-temperature properties for easier shifting in cold weather
  • Good seal compatibility
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Brookfield Viscosity
  • Viscosity Measurement, Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point, COC
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.