FM 1239 is a halogen free bedding compound for cable and wire with maximum 90ºC operating temperature at conductor and Insulation: 2 XI 1 XLPE (acc. DIN/VDE 0207 Part 22), or 2 YI 1-5 PE (acc. DIN/VDE 0207 Part 2), or 9YI 1 PP (acc. DIN/VDE 0207 Part 7), or 3GI 3 EPR (acc. DIN/VDE 0207 Part 20); and Sheathing: HM 4-2 HFFR (acc. DIN/VDE 0207 Part 24), or 2 YM 3 HDPE (acc. DIN/VDE 0207 Part 3); and other standards. Flame retardant; XLPE, PE, PP, EPR Insulation: HFFR, PE Sheathing. Applications: Market: PolyOne First ChoiceInformation provided by PolyOne Corporation. |