Polymist® F284 R is a white micronized PTFE powder composed of discrete particles. Available worldwide, Polymist® F284 R is a medium molecular weight grade with excellent thermal stability, designed for use in critical high temperature engineering and high performance polymers. As with all Polymist® micronized powders, F284 R offers excellent chemical and temperature residence, low surface energy, low coefficient of friction and good dispersion ability.Main features of Polymist® F284 R are: - Better wear resistance - Increased pressure x velocity (PV) limits - Reduced friction - Improved stick-slip response - Improved mold release Applications: Additive Storage and Handling - The usual precautions for safe storage and handling of Polymist® F284 R should be taken according to material safety documentation and experience. There will be no chemical deterioration of the Polymist® F284 R during proper storage. - Shelf life of Polymist® F284 R micronized powders will vary depending upon whether the recommended storage conditions are maintained and whether the material remains free from foreign contamination during storage time (not exposed to dirt, dust, water or other chemicals). The material should remain sealed in the original containers and storage conditions should provide for protection from temperature extremes as well as rain, snow or other wet environments (or such conditions which may damage the storage containers in which the product is stored). Safety and Toxicology - Before using Polymist® F284 R PTFE micronized powders, consult the product Material Safety Data Sheet and follow all label directions and handling precautions. - As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. - Do not smoke in areas contaminated with powder, vapor or fumes. - See Material Safety Data Sheet for detailed advice on waste disposal methods. Packaging - Polymist® F284 R is packaged in 25 kg nonreturnable drums. Each drum has two bag liners made of polyethylene resin. Information provided by Solvay Specialty Polymers. |