MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Flame Retardant adhesives
Master Bond MasterSil 707FR-NV One Component Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Key Features:
  • Passes UL 94V-1 and 94V-0 tests
  • Very fast cure
  • Non-corrosive
  • Superior adhesion properties
Product Description: MasterSil 707FR-NV is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It passes UL testing with a flame classification for 94V-1 for thicknesses of 0.75 mm and 1.5 mm, and 94V-0 for a 3 mm thickness. It adheres well to a wide variety of substrates including glass, metals and many plastics. The rapidity of the cure depends on the thickness of the layer and the humidity; the thicker the layer the slower the cure. It is exceptionally soft with superb elasticity and flexibility, and outstanding electrical insulation properties. Most importantly, it is non-corrosive, fast setting, and has a paste like consistency. MasterSil 707FR-NV is serviceable over the broad temperature range of -45°C to +105°C, as per UL specifications, and is gray in color.

Information provided by Master Bond, Inc.

Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength
  • Elongation at Break
  • Adhesive Bond Strength, lap shear, aluminum to aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94
  • Cure Time, Tack-free time
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Flame Retardant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.