MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Saint-Gobain Norton® MFA Fluoropolymer Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer

Material Notes:
  • Outstanding clarity
  • Performance from -254°C (-425°F) to 230°C (446°F)
  • Outstanding flex life and stress-crack resistance
  • Outstanding anti-stick release properties
  • Excellent electrical properties
  • Excellent weatherability
  • Minimum thicknesses of 0.0005" (0.0127 mm)
  • Widths up to 62" (1575 mm)
  • All films are manufactured and converted in class 100,000 clean room facility

Norton® MFA fluoropolymer film is manufactured from a semi-crystalline thermoplastic fluoropolymer (Hyflon® MFA, made by copolymerization of tetrafluoroethylene and perfluoromethyl vinyl ether) designed specifically for high temperature applications in the chemical and electrical industries. This film's unique properties place its performance between that of Norton® FEP and Norton® PFA films. Norton MFA film is a clear, transparent product that can be heat sealed, thermoformed, welded, metallized, or laminated to a wide variety of materials.

Norton MFA film offers a combination of excellent dielectric properties across a wide temperature and frequency range, chemical and stress-crack resistance similar to PFA, a continuous service temperature of 230° (446°F) and the highest clarity of any fluoropolymer film.

Chemical applications such as tank linings and roll covers benefit from this unique combination of properties.

The high clarity/low haze structure provides excellent performance in applications such as solar collectors, cell culture bagsm UV sterilization applicatios, and protective films from UV sources.

The combination of chemical resistance and high temperature resistance over a wide frequency range make Norton MFA film an ideal component for circuit board fabricators. Flat cable and electrical insulation applications benefit from the low dielectric constant and dissipation factors. Films are available from 0.0005" thickness up to 62" wide and are produced in a Class 100,000 clean room.

The high temperature resistance and non-wetting surface of Norton MFA make an ideal material for use as a high temperature release or bagging film for composite manufacturers. Norton MFA with 350-400% elongation, continuous service temperature of 230°C (446°F), and a melt point of 290°C (554°F) meet the needs of BMI systems requiring a 230°(446°F) cure temperature.

Surface Treatments Available: C-Treatable (cementable, 1 or 2 sides); Corona Treatment (1 or 2 sides); Chemical Etching (1 or 2 sides)
Flammability (UL-94) = V-0

Applications Include: Used for Aerospace/Release Films, Chemical Process, Electrical/Electronics, Medical, Protective/Decorative.

Specification Notes: All values represent typical performance properties and should not be used for specification purposes.
Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Specific Gravity, ASTM D-792
  • Water Absorption
  • Tensile Strength, Yield, ASTM D-882
  • Elongation at Break, ASTM D-882
  • Tensile Modulus, ASTM D-882
  • Surface Resistivity per Square, ASTM D-257
  • Dielectric Constant, ASTM D-150
  • Dielectric Strength, ASTM D-149, Value for a 1 mil sample.
  • Dissipation Factor, ASTM D-150
  • CTE, linear, ASTM D-696
  • Melting Point, ASTM D-3418
  • Maximum Service Temperature, Air, UL-746 B
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Refractive Index, ASTM D542
  • Haze, ASTM D1003
  • Transmission, Visible, transparent; thickness not quantified
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.