MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Morgan Advanced Ceramics Pyro-Log Fiber and Pyro Packaging R Grade Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Pyro-Log is an uncompressed monolithic mass of ceramic fiber. Pyro-Log fiber is available in 6" and 8" (152 mm and 203 mm) thicknesses with densities up to 15 pcf (240 kg/m3 ). Manufactured in three ceramic fiber grades, R, ZR and C, the Pyro-Log fiber can be used in a wide range of applications. Pyro-Log fiber is the basic building block for all Pyro-Bloc applications. All Pyro-Log fiber is produced with a special lubricant that allows the fibers to be intensely needled to attain densities up to 15 pcf. This lubricant also adds pliability which allows true multi-directional compression during installation. At moderate temperatures this lubricant burns out and the fiber mass becomes rigid. This feature, unique to Pyro-Log fiber, assists during installation and provides the durability and toughness necessary for long life.

Applications:

  • Low mass kiln cars
  • Fired heater floors
  • Back up insulation for insulating firebrick and castable lining
  • Fill gaps or small spaces where standard shapes are not practical

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density
  • Density
  • Density
  • Density
  • Thermal Conductivity, ASTM C201, at 160kg/m3
  • Thermal Conductivity, ASTM C201, at 160kg/m3
  • Thermal Conductivity, ASTM C201, at 160kg/m3
  • Thermal Conductivity, ASTM C201, at 160kg/m3
  • Melting Point
  • Maximum Service Temperature, Air, Continuous Use
  • Al2O3
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.