| Available Properties |
|---|
- Density, ISO 1183, DAM
- Water Absorption, Sim. to ISO 62, DAM
- Water Absorption, Sim. to ISO 62, DAM
- Moisture Absorption, Sim. to ISO 62, DAM
- Linear Mold Shrinkage, Flow, ISO 294-4, 2577, DAM
- Linear Mold Shrinkage, Transverse, ISO 294-4, 2577, DAM
- Hardness, Rockwell M, ISO 2039-2, DAM
- Tensile Strength at Break, ISO 527-1/-2, 50% RH
- Tensile Strength at Break, ISO 527-1/-2, DAM
- Elongation at Break, ISO 527-1/-2, DAM
- Elongation at Break, ISO 527-1/-2, 50% RH
- Tensile Modulus, ISO 527-1/-2, 50% RH
- Tensile Modulus, ISO 527-1/-2, DAM
- Flexural Strength, ISO 178, 50% RH
- Flexural Strength, ISO 178, DAM
- Flexural Modulus, ISO 178, 50% RH
- Flexural Modulus, ISO 178, DAM
- Compressive Strength, ISO 604, DAM
- Poissons Ratio, ISO 527-1/-2, DAM
- Shear Modulus, ASTM D 732, DAM
- Izod Impact, Notched (ISO), ISO 180/1U, 50% RH
- Izod Impact, Notched (ISO), ISO 180/1U, DAM
- Izod Impact, Notched (ISO), ISO 180/1U, DAM
- Izod Impact, Notched (ISO), ISO 180/1U, 50% RH
- Izod Impact, Unnotched (ISO), ISO 180/1A, 50% RH
- Izod Impact, Unnotched (ISO), ISO 180/1A, 50% RH
- Izod Impact, Unnotched (ISO), ISO 180/1A, DAM
- Izod Impact, Unnotched (ISO), ISO 180/1A, DAM
- Izod Impact, Unnotched (ISO), ISO 180/1A, DAM
- Izod Impact, Unnotched (ISO), ISO 180/1A, 50% RH
- Charpy Impact Unnotched, ISO 179/1eU, DAM
- Charpy Impact Unnotched, ISO 179/1eU, 50% RH
- Charpy Impact Unnotched, ISO 179/1eU, DAM
- Charpy Impact Unnotched, ISO 179/1eU, 50% RH
- Charpy Impact, Notched, ISO 179/1eA, 50% RH
- Charpy Impact, Notched, ISO 179/1eA, 50% RH
- Charpy Impact, Notched, ISO 179/1eA, DAM
- Charpy Impact, Notched, ISO 179/1eA, DAM
- Charpy Impact, Notched, ISO 179/1eA, DAM
- Charpy Impact, Notched, ISO 179/1eA, 50% RH
- Tensile Creep Modulus, 1 hour, ISO 899-1, 50% RH
- Tensile Creep Modulus, 1000 hours, ISO 899-1, 50% RH
- Abrasion, ISO 4649, mm3, DAM
- Volume Resistivity, IEC 62631-3-1, DAM
- Dielectric Constant, IEC 62631-2-1, DAM
- Dielectric Constant, IEC 62631-2-1, DAM
- Dissipation Factor, IEC 62631-2-1, DAM
- Dissipation Factor, IEC 62631-2-1, DAM
- Comparative Tracking Index, IEC 60112, DAM
- CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
- Specific Heat Capacity, Solid
- Specific Heat Capacity, Melt
- Thermal Conductivity, Melt
- Melting Point, ISO 11357-1/-3, 10°C/min; DAM
- Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2, DAM
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2, DAM
- Glass Transition Temp, Tg, ISO 11357-1/-2, 10°C/min; DAM
- Flammability, UL94, IEC 60695-11-10, DAM
- Flammability, UL94, IEC 60695-11-10, DAM
- Flame Spread, ISO 3795 (FMVSS 302)
- Oxygen Index, ISO 4589-1/-2, DAM
- Melt Temperature, Injection
- Melt Temperature, Injection Optimum
- Mold Temperature, Injection
- Mold Temperature, Injection Optimum
- Ejection Temperature, Injection
- Drying Temperature, Injection
- Dry Time, Dehumidified Dryer; Injection
- Moisture Content, Injection
- Hold Pressure, Injection
|
| | |