Properties: DINP is almost colourless and odorless oily liquid, free of foreign materials which is slightly soluble in water ( 0.285mg/L at 24°C ) but soluble in alcohols, hexane etc. It is miscible and compatible with all the monomeric plasticizers of PVC compounding. Application: Around 95% of DINP is used in PVC as a plasticizer. More than half of the remaining 5% is used in the production of polymers other than PVC (e.g. rubbers). The remaining DINP used in non-polymer application including anticorrosion paints, anti-fouling paints, lacquers, inks, adhesives and sealants. DINP is a monomeric primary plasticizers of medium molecular weight and fine performance. It has been developed to fulfill the need for an economical plasticizer in formulation which require very low volatility and good permanence characteristics. This products is widely used in vinylic compounds including wires, cables and plastisols. Chemical Name: DINP Molecular Formula: C 26 H42 O4 Molecular Structure: 26 H42 O4 CAS Number: 28553-12-0 EINECS NO.: 249-079-5 Information provided by KLJ Group |