Features: Autoclave Sterilizable; Ethylene Oxide Sterilizable; Good Processing Stability; High Clarity; High Purity; Kink Resistant; Radiation (Gamma) Resistant
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment
Agency Ratings: ISO 10993 Part 5
RoHS Compliance: RoHS Compliant
Form: Pellets
Processing Method: Injection Molding; Extrusion
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticThermoplastic Elastomer