Description: Apcoflex® N634E is a cold polymerized, medium ACN containing acrylonitrile butadiene co-polymer extended with 50 phr of non-DOP plasticizer. It contains non-staining antioxidant. Applications: Apcoflex® N634E is an medium viscosity plasticizer extended grade highly suitable for the manufacture of low durometer hardness products such as Printing Rolls, moulded components, Rubber Sponge and highly blown products. It is also recommended for applications in the manufacture of moulded and extruded goods where plasticiser free or low plasticizer extractions are desired. CAS No,: 9003-18-3 Information provided by Apcotex Industries Limited |