PARTITE 9330 a no-mixing, high viscosity combined with medium cure speed structural adhesive for wide variety of industrial assembly applications. It bonds wide range of materials with the use of Activator 1649. FEATURE: - Adhesive is applied to one surface and Activator to the other; press together and fixing is achieved within few minutes.
- Excellent resistance to gasoline, lubricants, water, solvents, etc.
APPLICATIONS:- Ideal for bonding Metals, Ferrite, Plated Metals, Ceramic, Wood, etc.
- Widely used for tool handle, electric motors, loudspeaker, decorative articles, sporting goods, appliances, etc.
Information provided by Parson Adhesives, Inc. |