MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Oxygen-free silver-bearing Copper, UNS C10500
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: auto gaskets, radiators, busbars, conductivity wire, contacts, radio parts, winding, switches, terminals, commutator segments, chemical process equipment, printing rolls, clad metals, printed circuit foil.

Available as flat products, rod, wire, tube and shapes. Similar alloys distinguished only by silver content: 8 oz/ton Ag (UNS C10400), 10 oz/ton Ag (UNS C10500), 25 oz/ton Ag (UNS C10700).

Key Words: AMSIL Copper; Oxygen-free Silver-Copper
Vendors:
Available Properties
  • Density, UNS C10700
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, silver free; wire cold worked 90% to a diameter of 2 mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.044 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.085 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.114 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.114 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.085 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.044 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, silver free; wire cold worked 90% to a diameter of 2 mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, silver free; wire cold worked 90% to a diameter of 2 mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.044 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.085 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.114 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.114 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.085 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.044 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, silver free; wire cold worked 90% to a diameter of 2 mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, silver free; wire cold worked 90% to a diameter of 2 mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.044 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.085 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.114 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.114 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.085 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.044 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, silver free; wire cold worked 90% to a diameter of 2 mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, silver free; wire cold worked 90% to a diameter of 2 mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.044 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.085 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.114 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.114 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.085 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.044 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, silver free; wire cold worked 90% to a diameter of 2 mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.044 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, silver free; wire cold worked 90% to a diameter of 2 mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.085 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Ultimate, 0.114 Ag; wire cold worked 90% to a diameter of 2mm and then annealed 1/2 h at various temperatures
  • Tensile Strength, Yield, Depending on temper
  • Elongation at Break, in 101.6 mm (4 in.)
  • Modulus of Elasticity
  • Poissons Ratio, Calculated
  • Machinability, UNS C36000 (free-cutting brass) = 100%
  • Forgeability
  • Shear Modulus
  • Electrical Resistivity, 100% IACS
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Annealing Point
  • Copper, Cu, Includes Ag
  • Silver, Ag, Min 10 troy oz./ton
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.