MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco Hydraulic Safety Fluid
Categories: Fluid; Lubricant

Material Notes: Texaco Hydraulic Safety Fluid is a fire-resistant fluid designed for use in high pressure hydraulic systems where the requirements for fire resistance, pump wear protection and viscosity are satisfied by water-glycol fluids.

Texaco Hydraulic Safety Fluid is a water solution of diethylene glycol containing antiwear agents and rust inhibitors.

Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  • Only distilled or deionized water should be used as makeup. The use of hard tap water, well or spring water should be avoided since the dissolved minerals in these waters will react with the additive system in the fluid to cause fluid haziness and formation of soap-like insoluble material.

    Fluid with a viscosity below 36.2 cSt at 40°C, or Brix readings below 42, contain excess water and only new Texaco Hydraulic Safety Fluid should be used as makeup.

CPS Number: 220766; MSDS Number: 10587

Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Moisture Content, vol% after makeup
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.