MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
PoolKemie SILIMOLD ADT-05 RTV2 silicon moulding rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Introduction: It is a two component room temperature vulcanizing pourable fluid silicon which cures on the addition of the appropriate CATALYST AD, according to the polyaddition process. SILIMOLD ADT 05 silicon rubber is characterized by its low hardness and no linear shrinkage.

Application: SILIMOLD ADT 05 silicon rubber is especially designed for heel inserts and inserts.

Peculiarities: Addition cure; Easy pour able; Faithfulness in details reproduction; Extreme mould release/mould life

Note 1: Tests have been carried out under these conditions: Temperature: +20°C; After: 24 ore; R.H.: 60%; Catalysis: 1:1

Information provided by Poolkemie

Vendors:
Available Properties
  • Viscosity, Comp. A, Before Catalysis, see note 1
  • Viscosity, Comp. B, Before Catalysis, see note 1
  • Linear Mold Shrinkage, ISO 4823, after 5 days ageing, After Catalysis
  • Storage Temperature
  • Hardness, Shore A, DIN 53505, After Catalysis
  • Cure Time, Demoulding time, See note 1, During Catalysis
  • Pot Life, See note 1, During Catalysis
  • Shelf Life, Both components (A and B) in their original tightly closed containers, in a dry and cool place , away from moisture
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.