| Notes: 90°C Insulation; RoHS Compliant Features: Flame Retardant Uses: Communication Wire Insulation Forms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; UL 13; UL 1424; UL 444 Wire Types: CL2R; CL3R; CMR; MPR; FPLR; OFNR Processing Method: Extrusion Additional Information: Temperature Rating: 90°C Information Provided by Teknor Apex |