MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Bethlehem Steel BETHSTAR Grade 50 1/4 to 2-1/2 in. thick, killed steel plate  (discontinued **)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Bethlehem's BethStar steels are proprietary grades of steel used for plates only. BethStar is produced as killed steel with fine grain practice, and is available in four strength levels. They are produced by a controlled-rolling process which results in plates having excellent formability, weldability, and impact toughness properties. Normal uses are demanding structural applications where strength to weight ratios are maximized. Frequently used as a replacement for some quenched and tempered steel plate grades. Its formability allows replacement of multi-piece weldments with formed parts.

Information provided by Bethlehem Steel Corporation

Data published in 1997. Bethlehem Steel in no longer in business.

Vendors:
Available Properties
  • Density, Typical of ASTM Steel
  • Hardness, Brinell, based on conversion from tensile strength
  • Hardness, Rockwell B, based on conversion from tensile strength
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break, in 8"
  • Bend Radius, Minimum, ASTM A6 PARA. S14, ≤1/4" W
  • Bend Radius, Minimum, ASTM A6 PARA. S14, >1/4 to 1" W
  • Bend Radius, Minimum, ASTM A6 PARA. S14, >1 to 2-1/2"W
  • Carbon, C
  • Iron, Fe
  • Manganese, Mn
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Bethlehem Steel Corporation

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.