Product Description: PP copolymer, 25% glass fiber, chemically coupled, colored upon request Different colors available: Scolefin 42 G 25-9: black; Scolefin 42 G 25-0: natural grade Availability: Europe; North America Filler/Reinforcement: Glass Fiber, 20% Filler by Weight Features: Chemically Coupled; Copolymer; Good Surface Finish Appearance: Black; Color Available; Natural color Information provided by Ravago Manufacturing Americas |