APTIV™ PEEK 2100 series films are the mineral filled amorphous films made from VICTREX™ PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications. APTIV PEEK 2100 has a unique combination of properties providing high temperature performance, light weight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen free and ease of processing makes APTIV films a technology enabler. APTIV PEEK 2100 series provides a higher modulus over the APTIV 2000 series amorphous films. This grade is tailored towards thermoforming of thin wall parts with higher modulus, such as speaker diaphragms. Applications: - Electrical Insulation
- Acoustic speaker diaphragms
- Thermoforming of thin wall parts
All information provided by Victrex. Properties measured on 50 micron film |