MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Osterman & Co OsterleneĀ® HD035-GP HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HD035-GP is designed for applications requiring excellent stiffness and stress crack resistant properties. It may be used as a sheet extrusion thermoforming resin or a general purpose blow molding resin. Suggested uses would include bottles and containers for bleach and detergents, personal care products and pharmaceutical packaging

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America
Features: Copolymer: High Density; High ESCR (Stress Crack Resist.); High Stiffness
Uses: Automotive Applications; Bottles; Containers; Packaging; Pharmaceutical Packaging
Processing Method: Blow Molding; Sheet Extrusion; Thermoforming

Information provided by Osterman & Company

Vendors:
Available Properties
  • Density, ASTM D792
  • ESCR 100% IgepalĀ®, ASTM D1693
  • Melt Flow, ASTM D1238
  • Tensile Strength, Yield, ASTM D638
  • 1% Secant Modulus, ASTM D790, Flexural
  • Tensile Impact Strength, ASTM D1822
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.