MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
ExxonMobil Bicor® 110 ASB-X OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. ASB-X is good for heavy dump VFFS applications (e.g., bulk tortillas) due to its excellent hot tack and seal strength. This film is suitable as an unsupported web or in a lamination. It can be surface printed, reverse printed or used unprinted.

Availability: Latin America, North America and South America

Key Features:

  • Outstanding optical properties
  • Robust machinability
  • Low and consistent COF
  • Excellent flavor and aroma barrier
  • Excellent heat seal strength and hot tack
  • Very good moisture barrier
  • Good Oxygen barrier
Features:
  • Acrylic Coated
  • Flavor & Aroma Barrier
  • Gas Barrier
  • In Lamination Lap sealable
  • Moisture Barrier
  • Oxygen Barrier
  • PVdC Coated
Applications:
  • Biscuits/Cookie/Crackers
  • Box Overwrap
  • Confectionery, Sugar
Uses:
  • Box Overwrap Flexible Packaging
  • HFFS Flexible Packaging
  • Pre-made Bags - Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Out Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing.

Information provided by ExxonMobil Chemical

Vendors:
Available Properties
  • Water Vapor Transmission, ExxonMobil Method, 90% RH
  • Oxygen Transmission Rate, ExxonMobil Method, 23°C, 0% RH
  • Thickness, ExxonMobil Method, Nominal
  • Coating Weight, ExxonMobil Method
  • Coefficient of Friction, ExxonMobil Method
  • Film Tensile Strength at Break, MD, ExxonMobil Method
  • Film Tensile Strength at Break, TD, ExxonMobil Method
  • Shrinkage, MD, ExxonMobil Method
  • Shrinkage, TD, ExxonMobil Method
  • Haze, ExxonMobil Method
  • Gloss, ExxonMobil Method, 45º
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.