MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
ExxonMobil Escorene® UL 8705 Adhesive Application Resin
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Escorene Ultra UL 8705 is a relatively low viscosity, 27.6% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has good compatibility with both hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt adhesives, glue sticks, sealants and wax blends.

Availability: Asia Pacific, Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Adhesives and Sealants
  • Glue Sticks
  • Industrial Sealants
  • Low Viscosity Adhesives
Information provided by ExxonMobil Chemical

Vendors:
Available Properties
  • Density, ExxonMobil Method
  • Viscosity, ASTM D3236
  • Vinyl Acetate Content, ExxonMobil Method
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ASTM D2240, 15s
  • Hardness, Shore D, ASTM D2240, 15s
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Modulus, 1% Secant, ASTM D790
  • Melting Point, ExxonMobil Method, Peak Melting Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.