Homopolymer Applications: Nonwovens and Thin Walled Injection Molding Formolene 4101T is a low viscosity, highly isotactic polypropylene homopolymer designed primarily for Nonwovens and Thin Walled Injection Molding. It contains a unique combination of stabilizers which give it excellent gas fading resistance, mild UV resistance and appropriate process stability. Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact. Specimens were injection molded according to the conditions specified in ASTM D4101. Information provided by Formosa Plastics Corporation, USA. |