MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
ChevronTexaco Open Gear Grease
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.

Chevron Open Gear Greases contain special functional fillers such as molybdenum disulfide and graphite, which impart a long-lasting film on working surfaces. They also contain tackiness additives, wetting agents and rust inhibitors to protect metal surfaces. None of the Chevron Open Gear Greases contain chlorinated solvents. Chevron Open Gear Greases have been formulated with a diluent that does not require a cancer warning label.

Chevron Open Gear Greases are in every sense true greases and not asphalt-based open gear lubricants. This has a number of advantages. The lubricants can carry a more complete additive system including friction modifiers such as molybdenum disulfide and graphite, which apply a long lasting antiwear film on gear teeth.

Applications

Chevron Open Gear Greases are recommended:

  • for all open gears in industrial, mining, construction, and marine equipment
  • for chain and sprocket lubrication
  • as a tenacious fifth wheel lubricant
Chevron Open Gear Greases can be applied in a variety of methods, including:
  • from a cartridge in a caulking gun
  • from an aerosol can for easy application in hard-toreach lubrication points
  • through a mechanical lubricator over a wide range of operating temperatures

Key Words: CPS Number: 230002; MSDS Number: 6809
Vendors:
Available Properties
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Penetration P(0), 1/10 mm
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.