MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Hexcel® HexWeb® HRH-327 - 3/16 - 4.0 Fiberglass Reinforced Polyimide Honeycomb
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Polyimide, TS

Material Notes: Designation: Material-Cell Size (inches)-Density
HexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well as both the initial and final web impregnations. This material has been developed for extended service temperatures up to 500°F with short-term capabilities up to 700°F. Unless other specified, material will have standard postcure.

Features: High-strength retention up to 500°F continuous service; 700°F short and intermittent term exposures; All polyimide resin and adhesive system; Good dielectric properties; Good insulative properties; Compatible with Hexcel polyimide adhesive, foam, and prepreg.
Applications: A high-temperature nonmetallic honeycomb for use in sandwich structures that require good electrical properties or that see service temperatures in the range of 350°F-500°F. Applications include sandwich structures for Mach 2 and Mach 3 aircraft, high-energy radomes, structural and acoustical engine inlets and liners.

Vendors:
Available Properties
  • Density
  • Compressive Yield Strength, Stabilized, min, preliminary value obtained at .500 inch thickness
  • Compressive Yield Strength, Stabilized, typical, preliminary value obtained at .500 inch thickness
  • Compressive Modulus, Stabilized, typical, preliminary value obtained at .500 inch thickness
  • Shear Modulus, Plate Shear, W Direction, typical, preliminary value obtained at .500 inch thickness
  • Shear Modulus, Plate Shear, L Direction, typical, preliminary value obtained at .500 inch thickness
  • Shear Strength, Plate Shear, W Direction, min, preliminary value obtained at .500 inch thickness
  • Shear Strength, Plate Shear, W Direction, typical, preliminary value obtained at .500 inch thickness
  • Shear Strength, Plate Shear, L Direction, min, preliminary value obtained at .500 inch thickness
  • Shear Strength, Plate Shear, L Direction, typical, preliminary value obtained at .500 inch thickness
  • Maximum Service Temperature, Air, Extended
  • Maximum Service Temperature, Air, Short Term
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.