MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
ChevronTexaco Spindura® 22
Categories: Fluid; Lubricant

Material Notes: Texaco Spindura oils deliver value through:
  • High oxidation stability — Longer service life than with conventional lubricants.
  • Rust and corrosion protection — Gives excellent protection against corrosion of both copper and steel.
  • Foam inhibition — Contains special foam suppressant. Eliminates both foaming and aeration problems.
  • Excellent antiwear properties — Maximizes spindle life by controlling wear.
  • Fast water separation — Minimize rust problems by fast release of water.

Texaco Spindura oils are premium oils manufactured especially to meet the severe requirements of spindle lubrication.

They provide excellent antiwear protection, oxidation and corrosion inhibition, as well as foam suppression.

Texaco Spindura oils are designed for use:

  • In machine tool spindles
  • Textile applications

Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220788; MSDS Number: 8640

Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.