MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Norplex-Micarta NP130HF Epoxy Glass Laminate Sheet, NEMA FR-4
Categories: Polymer; Thermoset; Epoxy

Material Notes: NP130HF is a woven glass fabric composite combined with epoxy resin system, which is engineered to provide better physical properties than standard NEMA FR-4. It is significantly more dimensionally stable than NP130 or NP510A because of its low resin content. The main application for NP130HF is for “bed-of-nails” probe boards used for printed circuit board testing, and other structural applications.

Information provided by Norplex-Micarta

Key Words: Glass Fiber, Epoxy, Micarta, NEMA FR-4, ASTM D709 Type IV Grade FR-4, MIL-I-24768/27 GEE-F, IPC 4101/21
Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM D570 Condition A
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, ASTM D638 Condition A, CrossWise
  • Tensile Strength, ASTM D638 Condition A, LengthWise
  • Flexural Strength, ASTM D790 Condition A, CrossWise
  • Flexural Strength, ASTM D790 Condition A, LengthWise
  • Flexural Modulus, ASTM D790 Condition A, CrossWise
  • Flexural Modulus, ASTM D790 Condition A, LengthWise
  • Compressive Strength, ASTM D695 Condition A, Flatwise
  • Shear Strength, ASTM D732 Condition A, perpendicular
  • Izod Impact, Unnotched, ASTM D256 Condition E-48/50, CrossWise
  • Izod Impact, Unnotched, ASTM D256 Condition E-48/50, LengthWise
  • Dielectric Constant, ASTM D150 Condition D-24/23
  • Dielectric Strength, ASTM D149 Condition D-48/50
  • Dielectric Strength, ASTM D149 Condition A
  • Dielectric Breakdown, ASTM D149 Condition D-48/50
  • Dielectric Breakdown, ASTM D149 Condition A
  • Dissipation Factor, ASTM D150 Condition D-24/23
  • Arc Resistance, ASTM D495 Conition A
  • Comparative Tracking Index, ASTM D3638
  • CTE, linear, Parallel to Flow, IPC-TM 650-2.4.24
  • CTE, linear, Transverse to Flow, IPC-TM 650-2.4.24
  • Transformation Temperature, Tg, DMA
  • UL RTI, Electrical, UL Bulletin 746b
  • UL RTI, Mechanical with Impact, UL Bulletin 746b
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.