MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Go Yen Chemical GOYENCHEM-ADC-108 Blowing Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Characteristic:
  • Excellent foaming ability
  • The series products can be used in various application after special dispersal process.
  • It can be used in normal atmospheric pressure foaming and pressure foaming
  • Thin powder
  • It could get white plastic foam.
  • Great resiliency.
  • It gives end-products even and solid foaming structure.
Applications:
  • It mainly use in PVC.
  • polyethylene, polypropylene, polystyrene
  • polyamide, nylon-6, ABS resin
  • rubber system : chloroprene rubber, acrylonitrilebutadiene rubber, natural rubber, butyl rubber, styrenebutadiene rubber, silicone rubber. Foaming processing of chloroprene rubber and various synthetic materials.
  • various thermosetting resin: PU, UP, acrylic
  • high foaming slice products
  • It’s suitable for producing high valued foaming synthetic leather
  • other special applications

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Particle Size, fineness 96%
  • Ash
  • Decomposition Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.