Good to excellent corrosion resistance. Good hot and cold formability. Applications: high-strength constructional parts for sea water corrosion resistance, hydrophone cases, mooring cable wire, springs, retainer rings, bolts, screws, pins for ocean telephone cable applications. Available as flat products, rod and wire. |