Parco Lubrite 2 is formulated to produce nonmetallic, oil-absorptive coatings on iron and steel bearing surfaces. These corrosion-resistant coatings consist chiefly of iron and manganese phosphates, and reduce wear on such articles as pistons, rings, liners, camshafts, tappets, motor blocks and similar bearing surfaces. Application: Magnesium Phosphate Conversion Coating |
Aerospace Surface Treatment |