Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is available in natural, heat stabilized and pigmented versions. It combines good strength, stiffness, and toughness as well as excellent heat, chemical and abrasion resistance. Applications: gears, fittings, casters, bearings, clips, fasteners, plugs, caps, and filter bowls. Information provided by BASF |