MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Eastman Kristalex™ 3105SD Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Kristalex™ 3105SD Hydrocarbon Resin is a water clear, highly color stable, nonpolar, low molecular weight thermoplastic polymer with low organic volatile content. This resin is compatible with a wide variety of oils, waxes, alkyds, plastics, and elastomers, and is soluble in many common organic solvents. It is indicated for use in plastics modification, adhesives, coatings, sealants, and caulks. In EVA-based hot melt adhesives Kristalex™ 3105SD is compatible with EVA grades with up to 18% vinyl acetate and is useful in formulating low-color, low odor adhesives with good low temperature properties. In styrenic block copolymer based adhesives Kristalex™ 3105SD preferentially associates with the styrenic endblocks, producing higher room-temperature cohesion without affecting tack and adhesion properties. Kristalex™ 3105SD complies with many FDA regulations for applications involving food contact. Users of this product should determine its compliance for their specific application prior to use.

Application/Uses:

  • Alluminum-pigment preparations
  • Assembly
  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Hot Melt Adhesives
  • Laminating
  • Nonwovens
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
Key Attributes:
  • Excellent thermal stability
  • Intermediate softening point
  • Low organic volatile content
  • Made from purified aromatic monomers
  • Suitable for use in food contact applications
  • Water-white initial color

Information provided by Eastman

Vendors:
Available Properties
  • Viscosity, Melt
  • Viscosity, Melt
  • Viscosity, Melt
  • Viscosity, Melt
  • Molecular Weight, Mz
  • Molecular Weight, Mw. Mw/Mn ratio = 1.8
  • Molecular Weight, Mn
  • Glass Transition Temp, Tg
  • Ring & Ball Softening Point, ASTM E 28
  • Gardner Color Number, ASTM D6166
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.