Hyflon® MFA P6010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in antistick applications. Hyflon® MFA P6010 exhibits very low surface energy, very low coefficient of friction, excellent optical properties and outstanding thermal and flame resistance. Additionally Hyflon® MFA P6010 coatings show excellent smooth surface finish, optimum antistick behavior and can maintain performance over a wide temperature range. Main features of Hyflon® MFA P6010 include: - Optimum antistick behavior - Very low coefficient of friction - Excellent surface finish - Excellent thermal resistance Good Optical Properties; Good Surface Finish; Good Thermal Stability; Low Friction; Semi Crystalline Uses: Coating Applications Processing: Coating Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Information provided by Solvay Specialty Polymers. |