Available Properties |
---|
- Density, ASTM D1505
- Density, ASTM D792
- Water Absorption, ASTM D570, immersion
- Water Vapor Transmission, ASTM F1249
- Oxygen Transmission, ASTM D3985
- Carbon Dioxide Transmission, ASTM D1434
- Thickness, ASTM D374
- Hardness, Rockwell R, ASTM D785
- Tensile Strength at Break, ASTM D638
- Film Tensile Strength at Yield, MD, ASTM D882
- Film Tensile Strength at Yield, TD, ASTM D882
- Tensile Strength, Yield, ASTM D638
- Film Elongation at Break, MD, ASTM D882
- Film Elongation at Break, TD, ASTM D882
- Film Elongation at Yield, MD, ASTM D882
- Film Elongation at Yield, TD, ASTM D882
- Elongation at Break, ASTM D638
- Tensile Modulus, ASTM D882, MD
- Tensile Modulus, ASTM D882, TD
- Tensile Modulus, ASTM D638
- Flexural Yield Strength, ASTM D790
- Flexural Modulus, ASTM D790
- Izod Impact, Notched, ASTM D256
- Izod Impact, Notched, ASTM D256
- Izod Impact, Unnotched, ASTM D4812
- Izod Impact, Unnotched, ASTM D4812
- Izod Impact, Unnotched, ASTM D4812
- Izod Impact, Unnotched, ASTM D4812
- Puncture Energy, ASTM D3763, Energy @ Max. Load, 2.5 mm (0.100 in.) Thick Plaques
- Puncture Energy, ASTM D3763, Energy @ Max. Load, 3.2 mm (0.125 in.) Thick Plaques
- Puncture Energy, ASTM D3763, Energy @ Max. Load, 2.5 mm (0.100 in.) Thick Plaques
- Puncture Energy, ASTM D3763, Energy @ Max. Load, 3.2 mm (0.125 in.) Thick Plaques
- Tear Strength, Total, ASTM D2582, MD, PPT Tear Resistance
- Tear Strength, Total, ASTM D2582, TD, PPT Tear Resistance
- Tear Strength, ASTM D1938, MD, Tear Propagation Resistance, Split Tear Method @ 254 mm/min (10 in./min)
- Tear Strength, ASTM D1938, TD, Tear Propagation Resistance, Split Tear Method @ 254 mm/min (10 in./min)
- Tear Strength, ISO 6383-1, MD, Trouser @ 200 mm/min
- Tear Strength, ISO 6383-1, TD, Trouser @ 200 mm/min
- Elmendorf Tear Strength MD, ASTM D1922
- Elmendorf Tear Strength TD, ASTM D1922
- Dart Drop Test, ASTM D1709A Modified
- Dart Drop Test, ASTM D1709A Modified
- Film Tensile Strength at Break, MD, ASTM D882
- Film Tensile Strength at Break, TD, ASTM D882
- Volume Resistivity, ASTM D257
- Surface Resistivity per Square, ASTM D257
- Dielectric Constant, ASTM D150
- Dielectric Constant, ASTM D150
- Dielectric Strength, ASTM D149, Short Time, 500 V/sec rate-of-rise
- Dissipation Factor, ASTM D150
- Dissipation Factor, ASTM D150
- Arc Resistance, ASTM D257
- CTE, linear, ASTM D696
- Specific Heat Capacity, DSC
- Specific Heat Capacity, DSC
- Specific Heat Capacity, DSC
- Specific Heat Capacity, DSC
- Specific Heat Capacity, DSC
- Thermal Conductivity, ASTM C177
- Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
- Vicat Softening Point, ASTM D1525
- Glass Transition Temp, Tg, DSC
- Haze, ASTM D1003
- Transmission, Visible, ASTM D1746, Transparency
- Transmission, Visible, ASTM D1003 Modified, Regular
- Transmission, Visible, ASTM D1003 Modified, Total
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- USP Class VI, See notes for details
|
| | |