MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Röhm ACRYLITE® Film Yellow 1F006 PMMA  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: PLEXIGLAS® Film 1F006 is a yellow transparent weather resistant acrylic film, especially developed for laminates. The film shows an excellent performance in longtime outdoor weathering. It provides high protection of laminating systems from degradation caused by UV radiation. Its very smooth surface leads the film to have an excellent optical and flatness quality surface.

Application PLEXIGLAS® Film 1F006 is recommended for traffic control signs according to different standards like DIN 6171-1 and ASTM D4956-01. PLEXIGLAS® Film 1F006 can be laminated on different polymeric films and sheets. Laminated decoration films based on PLEXIGLAS® are suitable for a wide range of molding processes such as thermoforming, and insert molding. Due to its good optical property and lamination behavior with pressure sensitive adhesive (PSA), PLEXIGLAS® Film 1F006 can be used as overlay laminates for reflective products for traffic control and guidance signs.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors:
Available Properties
  • Density, DIN 53479
  • Surface Tension, DIN 53364
  • Tensile Strength, Yield, ISO 527-3
  • Elongation at Break, ISO 527-3
  • Elongation at Yield, ISO 527-3
  • Glass Transition Temp, Tg, ISO 11357
  • Refractive Index, ISO 489
  • Transmission, Visible, ISO 13458-2
  • UV Transmittance, DIN EN 410
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Röhm GmbH , former product of Evonik Corporation; Evonik Cyro

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.