MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Telles Mirel™ P1001 Bioplastic, Injection Molding Grade  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: Mirel™ P1001 is a high performance, semi-crystalline polyester specifically engineered for high modulus injection molding applications. Mirel resins are innovative and solutions suitable for a wide variety of applications.

Environmental Innovation: Environmental responsibility is a major trend among industry leading brand owners and OEMs. Mirel is a new family of biobased resin providing the industry with sustainable alternatives to conventional plastics. Mirel meets the demands of environmentally-conscious companies and consumers making a positive impact on global climate change. Mirel starts with nature and ends with nature. It harmlessly biodegrades in all of these environments:

  • Industrial and home composting
  • Soil
  • Municipal waste treatment facilities, septic systems
  • Wetlands, streams, and oceans.

Potential Applications:

  • Food service ware-Single serve containers, caps, lids and trays
  • Consumer and packaging - Cosmetic cases and lipsticks.
Product Attributes
  • High modulus
  • Heat resistance
  • High gloss
  • Easy Processing
Biodegradation Certifications and Testing: Mirel resins are certified to ASTM D6400 / EN 13432 for compostable plastics, and D7081 / EN 17556 for non-floating biodegradable plastics in marine environment. Test results from ASTM D5988-96 / ISO 17556 for aerobic biodegradation in soil of plastics or residual plastics materials show that Mirel fully biodegrades - fungal/bacterial under ambient conditions. Test results from ASTM D5209 / ISO 14852 / ASTM D5271 / 14851 for aerobic biodegradation of plastic materials in an activated-sludge wastewater-treatment system show that fully biodegrades - bacterial under ambient conditions.

Property data listed measured after 21 day aging.

Telles is a joint venture between Metabolix and Archer Daniels Midland Company.

Key Words: Polyhydroxyalkanoate
Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570, 24 hrs
  • Viscosity, ASTM D3835
  • Linear Mold Shrinkage, ASTM D955
  • Tensile Strength, Yield, ISO 527-1, -2
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Break, ISO 527-1, -2
  • Flexural Strength, ISO 178
  • Flexural Strength, ASTM D790 A
  • Flexural Modulus, ASTM D790 A
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched, ASTM D256 A
  • Izod Impact, Notched (ISO), ISO 180 A
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1 B
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648 B
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1 A
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648 B
  • Vicat Softening Point, ASTM D1525 A10
  • Vicat Softening Point, ISO 306 A50
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature, Note reverse temperature profile
  • Nozzle Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Back Pressure, (Low) (Melt)
  • Screw Speed, (Slow)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Metabolix (Telles)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.