MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
DuPont Mobility and Materials Zytel® (PA612) FG158 NC010 PA612  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: Unreinforced Polyamide 612 Developed for Food Contact Applications

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors:
Available Properties
  • Density, ISO 1183, DAM
  • Melt Density
  • Water Absorption, Sim. to ISO 62, DAM
  • Moisture Absorption, Sim. to ISO 62, DAM
  • Viscosity Number, ISO 307, 1157, 1628, DAM
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577, DAM
  • Linear Mold Shrinkage, Flow, DAM
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577, DAM
  • Linear Mold Shrinkage, Transverse, DAM
  • Hardness, Rockwell R, ISO 2039-2, 50%RH
  • Hardness, Rockwell R, ISO 2039-2, DAM
  • Tensile Strength, Yield, ISO 527-1/-2, 50%RH
  • Tensile Strength, Yield, ISO 527-1/-2, DAM
  • Film Elongation at Yield, MD, ISO 527-3, DAM
  • Elongation at Break, ISO 527-1/-2, Nominal; DAM
  • Elongation at Break, ISO 527-1/-2, Nominal; 50%RH
  • Elongation at Yield, ISO 527-1/-2, DAM
  • Elongation at Yield, ISO 527-1/-2, 50%RH
  • Tensile Modulus, ISO 527-1/-2, 50%RH
  • Tensile Modulus, ISO 527-1/-2, DAM
  • Poissons Ratio, DAM
  • Poissons Ratio, 50%RH
  • Izod Impact, Notched (ISO), ISO 180/1A, DAM
  • Izod Impact, Notched (ISO), ISO 180/1A, 50%RH
  • Izod Impact, Notched (ISO), ISO 180/1A, DAM
  • Izod Impact, Notched (ISO), ISO 180/1A, 50%RH
  • Charpy Impact Unnotched, ISO 179/1eU, DAM
  • Charpy Impact Unnotched, ISO 179/1eU, 50%RH
  • Charpy Impact Unnotched, ISO 179/1eU, DAM
  • Charpy Impact Unnotched, ISO 179/1eU, 50%RH
  • Charpy Impact, Notched, ISO 179/1eA, 50%RH
  • Charpy Impact, Notched, ISO 179/1eA, DAM
  • Charpy Impact, Notched, ISO 179/1eA, DAM
  • Charpy Impact, Notched, ISO 179/1eA, 50%RH
  • Volume Resistivity, IEC 62631-3-1, 50%RH
  • Volume Resistivity, IEC 62631-3-1, DAM
  • Surface Resistance, IEC 62631-3-2, 50%RH
  • Dielectric Constant, IEC 62631-2-1, DAM
  • Dielectric Constant, IEC 62631-2-1, DAM
  • Dielectric Constant, IEC 62631-2-1, 100Hz; 50%RH
  • Dielectric Constant, IEC 62631-2-1, 100Hz; 50%RH
  • Dielectric Strength, IEC 60243-1, DAM
  • Dielectric Strength, IEC 60243-1, 50%RH
  • Dissipation Factor, IEC 62631-2-1, DAM
  • Dissipation Factor, IEC 62631-2-1, DAM
  • Dissipation Factor, IEC 62631-2-1, 50%RH
  • Dissipation Factor, IEC 62631-2-1, 50%RH
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
  • Specific Heat Capacity, Melt
  • Thermal Conductivity, Melt
  • Melting Point, ISO 11357-1/-3, 10°C/min; DAM
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2, DAM
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2, DAM
  • Vicat Softening Point, ISO 306, 50°C/h; DAM
  • Glass Transition Temp, Tg, ISO 11357-1/-2, 10°C/min; 50%RH
  • Glass Transition Temp, Tg, ISO 11357-1/-2, 10°C/min; DAM
  • Flammability, UL94, IEC 60695-11-10, DAM
  • Flammability, UL94, IEC 60695-11-10, DAM
  • Flame Spread, ISO 3795 (FMVSS 302)
  • Oxygen Index, ISO 4589-1/-2, DAM
  • Melt Temperature, Optimum, Extrusion
  • Melt Temperature, Extrusion
  • Melt Temperature, Optimum, Injection
  • Melt Temperature, Injection
  • Mold Temperature, Injection
  • Drying Temperature, Extrusion; Dehumidified Dryer
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.