MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
3M Scotch-Weld™ DP-105 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar surfaces where thermal coefficient of expansion may be a problem. It is also unique in that it retains its clear, colorless properties even when cured in larger masses where many clear epoxy systems will often turn amber from the reaction exotherm.

Information provided by 3M

Vendors:
Available Properties
  • Brookfield Viscosity, Base, RVF #7 spindle, 20 rpm @ 27°C
  • Brookfield Viscosity, Accelerator, RVF #7 spindle, 20 rpm @ 27°C
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D882
  • Elongation at Break, ASTM D882
  • Shear Strength, Overlap, Polypropylene
  • Shear Strength, Overlap, Glass, Borosilicate
  • Shear Strength, Overlap, +3M Primer 3901
  • Shear Strength, Overlap, Acrylic
  • Shear Strength, Overlap, Wood, Fir
  • Shear Strength, Overlap, ABS
  • Shear Strength, Overlap, Polycarbonate
  • Shear Strength, Overlap, PVC
  • Shear Strength, Overlap, Cold Rolled Steel
  • Shear Strength, Overlap, Fiberglass
  • Shear Strength, Overlap, Sanded Aluminum
  • Shear Strength, Overlap, Etched Aluminum
  • Shear Strength, Overlap
  • Shear Strength, Overlap
  • Shear Strength, Overlap
  • Shear Strength, Overlap
  • Shear Strength, Overlap
  • Peel Strength, 180°
  • Peel Strength, 180°
  • Peel Strength, 180°
  • Peel Strength, 180°
  • Peel Strength, 180°
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • CTE, linear
  • Thermal Conductivity, ASTM C177
  • Glass Transition Temp, Tg, Onset
  • Glass Transition Temp, Tg, Mid-Point
  • Cure Time, Handling Strength
  • Cure Time
  • Tack-Free Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.