MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors:
Available Properties
  • Density, Average value: 0.920 g/cc Grade Count:746
  • Brightness, Average value: 48.7 % Grade Count:3
  • Moisture Vapor Transmission, Average value: 0.404 cc-mm/m²-24hr-atm Grade Count:23
  • Water Vapor Transmission, Average value: 9.19 g/m²/day Grade Count:22
  • Water Vapor Transmission, Average value: 11.7 g/m²/day Grade Count:5
  • Oxygen Transmission, Average value: 201 cc-mm/m²-24hr-atm Grade Count:21
  • Oxygen Transmission Rate, Average value: 4500 cc/m²/day Grade Count:3
  • Environmental Stress Crack Resistance, Average value: 694 hour Grade Count:30
  • Environmental Stress Crack Resistance, Average value: 1000 hour Grade Count:5
  • Thickness, Average value: 31.0 microns Grade Count:388
  • Melt Flow, Average value: 2.52 g/10 min Grade Count:709
  • Base Resin Melt Index, Average value: 1.71 g/10 min Grade Count:16
  • Hardness, Shore D, Average value: 56.2 Grade Count:28
  • Tensile Strength, Ultimate, Average value: 27.1 MPa Grade Count:53
  • Film Tensile Strength at Yield, MD, Average value: 10.8 MPa Grade Count:378
  • Film Tensile Strength at Yield, TD, Average value: 10.9 MPa Grade Count:375
  • Tensile Strength, Yield, Average value: 12.7 MPa Grade Count:44
  • Film Elongation at Break, MD, Average value: 617 % Grade Count:673
  • Film Elongation at Break, TD, Average value: 813 % Grade Count:651
  • Film Elongation at Yield, MD, Average value: 193 % Grade Count:14
  • Film Elongation at Yield, TD, Average value: 275 % Grade Count:14
  • Elongation at Break, Average value: 692 % Grade Count:68
  • Modulus of Elasticity, Average value: 0.194 GPa Grade Count:36
  • Flexural Modulus, Average value: 0.347 GPa Grade Count:36
  • Secant Modulus, Average value: 0.199 GPa Grade Count:20
  • Secant Modulus, MD, Average value: 0.195 GPa Grade Count:506
  • Secant Modulus, TD, Average value: 0.223 GPa Grade Count:506
  • Izod Impact, Notched (ISO), Average value: 10.0 kJ/m² Grade Count:16
  • Charpy Impact, Notched, Grade Count:7
  • Puncture Energy, Average value: 2.97 J Grade Count:89
  • Coefficient of Friction, Average value: 0.502 Grade Count:193
  • Coefficient of Friction, Static, Average value: 0.714 Grade Count:5
  • Tear Strength Test, Average value: 20.0 Grade Count:6
  • Elmendorf Tear Strength MD, Average value: 238 g Grade Count:343
  • Elmendorf Tear Strength TD, Average value: 513 g Grade Count:346
  • Elmendorf Tear Strength, MD, Average value: 9.61 g/micron Grade Count:402
  • Elmendorf Tear Strength, TD, Average value: 21.6 g/micron Grade Count:401
  • Dart Drop, Average value: 8.74 g/micron Grade Count:344
  • Dart Drop Test, Average value: 251 g Grade Count:463
  • Seal Strength, Average value: 2070 g/25 mm Grade Count:12
  • Film Tensile Strength at Break, MD, Average value: 44.5 MPa Grade Count:685
  • Film Tensile Strength at Break, TD, Average value: 35.0 MPa Grade Count:664
  • Heat Seal Strength Initiation Temperature, Average value: 102 °C Grade Count:30
  • Melting Point, Average value: 120 °C Grade Count:220
  • Crystallization Temperature, Average value: 110 °C Grade Count:7
  • Vicat Softening Point, Average value: 103 °C Grade Count:190
  • Brittleness Temperature, Average value: -69.8 °C Grade Count:61
  • Haze, Average value: 12.6 % Grade Count:600
  • Gloss, Average value: 64.3 % Grade Count:582
  • Transmission, Visible, Average value: 86.0 % Grade Count:22
  • Processing Temperature, Average value: 219 °C Grade Count:65
  • Melt Temperature, Average value: 220 °C Grade Count:206
  • Die Opening, Average value: 0.165 cm Grade Count:54
  • Die Opening, Average value: 0.215 cm Grade Count:1
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.