A high crystallinity, high impact copolymer resin designed for injection molded applications requiring excellent processing attributes. Availability: Asia Pacific, North America. Features: balanced stiffness/toughness, good processability, nucleated, good impact resistance, heat aging resistant.. Applications: appliance components, automotive applications, industrial applications. Appearance: Natural Color. Forms: pellets. Processing Method: injection molding, compounding. Information provided by ExxonMobil. |
Achieve™ Advanced PP8285E1 |