MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
SABIC SABIC® COHERE™ S100L Metallocene Polyethylene (mPE) (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: SABIC® COHERE™ S100L is an ethylene-octene copolymers produced via solution polymerization using advanced metallocene catalyst. It performs well in high performance flexible packaging applications with excellent toughness, hot tack, hot seal, optical properties and enhanced packaging integrity to reduce loss/waste. It contains slip and antiblock additives.

Information provided by SABIC

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Film Elongation at Break, MD, ASTM D882, Properties have been measured by producing 40 µm film with 2.1 BUR, screw diameter 35mm, die diameter 100mm, die gap 1mm.
  • Film Elongation at Break, TD, ASTM D882, Properties have been measured by producing 40 µm film with 2.1 BUR, screw diameter 35mm, die diameter 100mm, die gap 1mm.
  • Elmendorf Tear Strength, MD, ASTM D1922, Properties have been measured by producing 40 µm film with 2.1 BUR, screw diameter 35mm, die diameter 100mm, die gap 1mm.
  • Elmendorf Tear Strength, TD, ASTM D1922, Properties have been measured by producing 40 µm film with 2.1 BUR, screw diameter 35mm, die diameter 100mm, die gap 1mm.
  • Dart Drop Test, ASTM D1709, Properties have been measured by producing 40 µm film with 2.1 BUR, screw diameter 35mm, die diameter 100mm, die gap 1mm.
  • Film Tensile Strength at Break, MD, ASTM D882, Properties have been measured by producing 40 µm film with 2.1 BUR, screw diameter 35mm, die diameter 100mm, die gap 1mm.
  • Film Tensile Strength at Break, TD, ASTM D882, Properties have been measured by producing 40 µm film with 2.1 BUR, screw diameter 35mm, die diameter 100mm, die gap 1mm.
  • 1% Secant Modulus, MD, ASTM D882, Properties have been measured by producing 40 µm film with 2.1 BUR, screw diameter 35mm, die diameter 100mm, die gap 1mm.
  • 1% Secant Modulus, TD, ASTM D882, Properties have been measured by producing 40 µm film with 2.1 BUR, screw diameter 35mm, die diameter 100mm, die gap 1mm.
  • Heat Seal Strength Initiation Temperature, SABIC method, Temperature at which 4 N/25.4mm heat seal strength is achieved.
  • Melting Point, SABIC method
  • Haze, ASTM D1003
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.