Borpact™ BC914TF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. This grade is especially developed for the manufacturing of unoriented film for various film processing technologies like cast film process, conventional blown film process with air cooling and roll stack process for thermoformable films/sheets. Optical properties will not be deteriorated as with conventional homo or copolymers at these temperatures. Applications: Borpact™ BC914TF is recommended for label film, lamination films, food packaging, map trays, stand up pouch film, vegetable trays, and inner layer in coextrusion.Information provided by Borealis AG |