MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
ChevronTexaco Taro® 16 XD SAE 30
Categories: Fluid; Lubricant

Material Notes: Texaco Taro 16 XD delivers value through:
  • Wear protection — Superior antiwear characteristics result in reduced wear on all moving engine components. Controls ring and liner wear through its ability to neutralize acids formed by the combustion of sulphur in fuel, permitting longer overhaul periods. High performance antiwear additives provide excellent protection for cams, camshaft and bearings.
  • Detergent/Dispersant properties — Prevents the formation of high temperature piston deposits, as well as low temperature sludge, in order to guarantee continuous oil flow inside the engine.
  • Oxidation stability — Provides a very high thermal and oxidation stability withstanding high thermal stresses of high output trunk piston engines and reducing undercrown deposits. Offers protection against liner lacquer formation,and is therefore suitable for use in low sulphur gas oil applications under high load conditions.
  • Rust protection — Formulated to provide excellent rust protection as required in stern tube applications.
  • Balanced additive combination — Ensures high quality performance with excellent overall protection. Provides minimum maintenance and down-time, long engine life and economical operating costs.

Texaco Taro 16 XD is a high performance medium alkaline diesel engine oil for medium and high-speed trunk piston diesel engines.

Texaco Taro 16 XD is a 16 base number oil, blended from carefully refined high quality base oils in combination with a specially developed package containing alkaline detergents, dispersants, oxidation and corrosion inhibitors, and antiwear agents.

Texaco Taro 16 XD is recommended for the lubrication of medium and high-speed turbo charged and naturally aspirated diesel engines, operating on gas oil and marine diesel oil containing low to medium sulfur levels (up to 1.8%).

Texaco Taro 16 XD is especially developed for marine and power generation applications. Texaco Taro 16 XD is highly suitable for applications which include a separator in the lubrication system. Texaco Taro 16 XD can be used in a multitude of applications such as reduction gears, air compressors, medium loaded gear applications, stern tubes, propulsion and auxiliary engines. This allows a reduction in the number of oils on board.

Texaco Taro 16 XD meets the requirements of the major high and medium-speed marine diesel engine manufacturers.

Texaco Taro 16 XD meets the performance requirements of API Service Category CF.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221676; MSDS Number: 8754

Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, Viscosity Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash, Sulfated Ash, mass %
  • Total Base Number, ASTM D2896
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.