Available Properties |
---|
- Volatiles
- Storage Temperature
- Tensile Strength, Flatwise, FM 94 co-cured with BMS 8-79 prepreg (epoxy/glass), BMS 8-124 core (Type 1, Class 1), Note 6
- Tensile Strength, Flatwise, 0.06 psf, Note 1
- Tensile Strength, Flatwise, CYCOM® 950-1 3K 70P 3 plies Composite surface preparation: nylon peel ply, Note 7
- Tensile Strength, Flatwise, CYCOM® 950-1 3K 70P 3 plies Composite surface preparation: nylon peel ply, Note 7
- Tensile Strength, Flatwise, Note 5
- Tensile Strength, Flatwise, Note 5
- Tensile Strength, Flatwise, 0.06 psf, Note 1
- Tensile Strength, Flatwise, 0.06 psf, Note 1
- Tensile Strength, Flatwise, 0.06 psf, Note 1
- Shear Strength, ASTM D3165, Wide Area Blister Detection, 0.06 psf, Note 1
- Shear Strength, CYCOM 985 3K 70P, 0.1 in (2.54 mm) thick, Note 7
- Shear Strength, FM 94M co-cured with CYCOM® 985 3K 70P (BMS 8-212 prepreg), Note 6
- Shear Strength, CYCOM 985 3K 70P, 0.1 in (2.54 mm) thick, Note 7
- Shear Strength, FM 94M co-cured with CYCOM® 985 3K 70P (BMS 8-212 prepreg), Exposure: 30 days at 160°F (71°C), 100% RH, Note 6
- Shear Strength, ASTM D3165, Wide Area Blister Detection, 0.06 psf, Note 1
- Shear Strength, CYCOM 985 3K 70P, 0.1 in (2.54 mm) thick, Note 7
- Shear Strength, ASTM D1002, 0.06 psf, Note 1
- Shear Strength, ASTM D3165, Wide Area Blister Detection, 0.06 psf, Note 1
- Shear Strength, FM 94M co-cured with CYCOM® 985 3K 70P (BMS 8-212 prepreg), Note 6
- Shear Strength, FM 94M co-cured with CYCOM® 985 3K 70P (BMS 8-212 prepreg), Exposure: 30 days at 160°F (71°C), 100% RH, Note 6
- Shear Strength, ASTM D1002, 0.06 psf, Note 1
- Shear Strength, ASTM D3165, Wide Area Blister Detection, 0.06 psf, Note 1
- Shear Strength, ASTM D3165, Wide Area Blister Detection, 0.06 psf, Note 1
- Shear Strength, ASTM D1002, 0.06 psf, Note 1
- Shear Strength, ASTM D1002, 0.06 psf, Note 1
- Peel Strength, ASTM D3167, Floating Roller, 0.06 psf, Note 1
- Peel Strength, ASTM D3167, Floating Roller, 0.06 psf, Note 1
- Peel Strength, ASTM D3167, Floating Roller, 0.06 psf, Note 1
- Peel Strength, ASTM D3167, Floating Roller, 0.06 psf, Note 1
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Shelf Life
|
| | |