MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco ISO 150 Utility Oil LVI
Categories: Fluid; Lubricant; Quenchant

Material Notes: Features

Chevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendencies and good natural film strength.

They can be used in circulating oil systems, low pressure hydraulics (< 1000 psi), and refrigeration compressor applications where low pour points and good oxidation stability are important considerations. Chevron Utility Oils LVI do an excellent job where customers desire a low cost product for noncritical applications.

Chevron Utility Oil LVI ISO 22 is also registered with NSF and is acceptable as a lubricant where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.

Applications

Chevron Utility Oils LVI are recommended for older industrial machinery using "once-through" lubricators such as bottle, wick, drip, sightglass feed, or wastepack oilers.

Chevron Utility Oil LVI ISO 22 has been used successfully as a quenching oil in some applications. Because of their high solvency, especially when heated, Chevron Utility Oils LVI ISO 22, 32, or 46 are ideal as engine or circulating system flushing oils, as they effectively remove lightly oxidized oil from system piping.

Chevron Utility Oil LVI ISO 46 performs well in hydraulic rams or lifts such as some car hoists in garages and service stations where pressures are low. This grade is also occasionally used in underground hydraulic mining equipment where ambient temperatures are low and the lubricant is frequently replenished.

There is ready separation from water provided by these oils. This is an important property where severe moisture conditions exist. Because of its low pour points, Chevron Utility Oil LVI ISO 46 isrecommended for use as refrigeration oils.

Chevron Utility Oil LVI ISO 100 is also recommended for use as compressor lubricants because of their low pour points and good oxidation stability.

Do not use Chevron Utility Oils LVI ISO 22, 32, or 46 in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Key Words: CPS Number: 231211; MSDS Number: 6887
Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.