Bapolan PS6045 is a high heat crystal polystyrene resin designed for fast cycle injection molding applications. This resin offers excellent clarity and heat distortion properties. It complies with US FDA 21CFR177.1640 and has a 94HB UL rating. Applications: Containers; Packaging. Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers |
Food Contact Acceptable; High Clarity |