MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Teknor Apex SarlinkĀ® TPV X5745B Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 5700B Series are highly engineered extrusion-grade thermoplastic vulcanizates with outstanding UV stability designed for demanding automotive interior and exterior sealing applications, including glass run channels, waistbelts, weather strips, seals and other profiles. This product is a medium hardness, low density, high performance grade with low fogging and excellent color retention and elastic properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: UV Stabilizer

Features: Chemical Resistant; Medium Hardness; Low Density; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Rubber Replacement

RoHS Compliance: RoHS Compliant

Automotive Specifications: DAIMLER DBL 5562.30 Color: Black; VAG VW501 23 Color: Black

Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ISO 1183
  • Viscosity, ASTM D3835, Shear, Capillary
  • Hardness, Shore A, ISO 868, Extruded
  • Hardness, Shore A, ISO 868, Injection Molded
  • Tensile Strength at Break, ISO 37, Flow
  • Tensile Strength at Break, ISO 37, Across Flow
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air at 168 hr
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air at 168 hr
  • Tensile Stress at Strain, ISO 37, Across Flow
  • Tensile Stress at Strain, ISO 37, Flow
  • Tensile Stress at Strain, ISO 188, Across Flow, Change in Air at 1000 hr
  • Tensile Stress at Strain, ISO 188, Across Flow, Change in Air at 168 hr
  • Elongation at Break, ISO 37, Flow
  • Elongation at Break, ISO 37, Across Flow
  • Elongation at Break, ISO 188, Across Flow, Change in Air at 168 hr
  • Elongation at Break, ISO 188, Across Flow, Change in Air at 168 hr
  • Tear Strength, ISO 34-1, Method Ba, Angle (Unnicked)
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.