MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
AGC Fluon® C-88AXMP ETFE
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Description: Fluon® ETFE is a melt-processable copolymer of tetrafluoroethylene and ethylene. Fluon ETFE possesses a unique combination of desirable properties such as higher resistance to heat and chemical attack and outstanding physical toughness. It is processable by conventional extrusion, injection molding, roto-molding, roto-lining, and electrostatic coating. It is available in a variety of forms including 1/8” pellets, designated as ‘P’, and powder, designated as ‘B’.

Benefits:

  • High resistance to heat: Fluon ETFE has a continuous use temperature of 150°C.
  • Excellent chemical resistance
  • Outstanding physical toughness: Fluon ETFE has better physical properties than most other fluoropolymers.
  • Low smoke and flame characteristics: Fluon ETFE is rated 94 V-0 by Underwriters Laboratories Inc.
  • Outstanding resistance to weather and aging
  • Good dielectric properties
  • Non-stick characteristics
Applications:
  • Wire & cable (automotive, industrial, aerospace, transit, and appliance markets)
  • Film and sheets
  • Tubing and pipe
  • Electronic components
  • Electrostatic and roto-molded vessel linings
  • Valves, fittings, and pump housings

Information provided by AGC Chemicals Americas Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow
  • Melt Flow, ASTM D3159
  • Melt Index of Compound, ASTM D1238
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Strength at Break
  • Tensile Strength at Break
  • Tensile Strength at Break
  • Tensile Strength, ASTM D638
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Flexural Strength, ASTM D790
  • Flexural Strength
  • Flexural Strength
  • Flexural Strength
  • Flexural Strength
  • Flexural Modulus, ASTM D790
  • Flexural Modulus
  • Flexural Modulus
  • Flexural Modulus
  • Flex Crack Resistance, ASTM D2176, Cycles per MIT Folding Endurance
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM C256
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, 10 mil film
  • CTE, linear, ASTM D696
  • Specific Heat Capacity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Brittleness Temperature, ASTM D764
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Mold Temperature
  • Injection Velocity
  • Injection Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Asahi Glass Company, AGC Fluorocompounds

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.