MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
DuPont Teijin Films Mylar® EC Polyester Film, 400 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outstanding durability, chemical inertness, good dielectrics, and good handling characteristics.

General Product Info: The outstanding strength, flexibility, and electrical properties of Mylar® EC films, combined with lower than normal shrinkage levels, make them especially suited for circuitry and membrane touch switch applications. The film's moisture and chemical resistance serve as a barrier to substances that could contaminate membrane touch switches.

Typical Applications: The unique balance of properties offered by Mylar® EC films makes them ideal for membrane switches and flexible circuits used in a variety of consumer and industrial products, including automotive instrument clusters, computers, calculators, telephones, cameras, and appliances.

Approvals: UL 94 VTM-2 - for 200 - 500 gauge (0.05 - 0.13mm)

Information provided by DuPont.

Vendors:
Available Properties
  • Density, ASTM D1505, Typical Mylar®
  • Thickness
  • Film Elongation at Break, MD, ASTM D882A
  • Film Elongation at Break, TD, ASTM D882A
  • Film Tensile Strength at Break, MD, ASTM D882A
  • Film Tensile Strength at Break, TD, ASTM D882A
  • Dielectric Strength, ASTM D149, 1/4" electrode 500 V/sec 25°C in air
  • Dielectric Breakdown, ASTM D149, 1/4" electrode 500 V/sec 25°C in air
  • Specific Heat Capacity, Typical Mylar®
  • Melting Point, Typical Mylar® via DSC
  • Shrinkage, MD, Unrestrained
  • Shrinkage, TD, Unrestrained
  • Refractive Index, typical of Mylar®
  • Haze, ASTM D1003
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DuPont Teijin Films

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.